Raw material preparation
Electron beam melting (EBM): Melting under 10⁻⁴ Pa vacuum to remove oxygen and nitrogen impurities to <50 ppm.
Zone melting (ZM): Purification by moving the heating zone, the impurity content is reduced to <1 ppm.
Forming process
Forging: temperature 1100-1250°C, deformation <30%, avoid grain coarsening.
Extrusion: Using glass lubricant, the extrusion ratio can reach 50:1, and Φ3-100 mm rods are produced.
Surface treatment
Anodizing: Generate 5-20 μm oxide film to improve corrosion resistance and bioactivity.
Physical vapor deposition (PVD): TiN coating, hardness increased to 2000 HV, wear resistance increased by 10 times.