Physical properties of molybdenum-copper alloy
1. Density and melting point: The density of molybdenum-copper alloy is 9.7g/cm³, and the melting point is about 2100℃.
2. Thermal expansion coefficient: The linear expansion coefficient of molybdenum-copper alloy is 6.8×10^-6/℃, which is relatively small, making it easy to heat seal.
3. Thermal conductivity: Molybdenum-copper alloy material has excellent thermal conductivity, up to 140W/(m·K), so it can conduct heat efficiently, making it widely used in the field of radiators.
Related parameters of molybdenum copper alloy
| Commodity Name | Copper molybdenum alloy |
| Grade | Mo85Cu15, Mo80Cu20, Mo70Cu30, Mo60Cu40, Mo50Cu50 |
| Density | 9.54-10g/cc |
| Property | High strength, good thermal and electrical conductivity, good high temperature resistance etc. |
| Specification | As per customer request or drawing |
| Production technique | Powder Metallurgy |
| Related products | Rod, sheet, plate, disk |
Our molybdenum copper alloy packaging and delivery
1) Wrap the board with paper, then plastic paper to prevent moisture
2) Foam board wraps the inner wooden box
3) The outside is a standard export plywood box
Delivery
Sample delivery: 7-10 days
Large order quantity: Usually we can supply within 20 days
Customer visit and company environment